Reliability of metalloceramic and zirconia-based ceramic crowns

N. R F A Silva, E. A. Bonfante, R. A. Zavanelli, V. P. Thompson, J. L. Ferencz, Paulo Coelho

Research output: Contribution to journalArticle

Abstract

Despite the increasing utilization of all-ceramic crown systems, their mechanical performance relative to that of metal ceramic restorations (MCR) has yet to be determined. This investigation tested the hypothesis that MCR present higher reliability over two Y-TZP all-ceramic crown systems under mouth-motion fatigue conditions. A CAD-based tooth preparation with the average dimensions of a mandibular first molar was used as a master die to fabricate all restorations. One 0.5-mm Pd-Ag and two Y-TZP system cores were veneered with 1.5 mm porcelain. Crowns were cemented onto aged (60 days in water) composite (Z100, 3M/ESPE) reproductions of the die. Mouth-motion fatigue was performed, and use level probability Weibull curves were determined. Failure modes of all systems included chipping or fracture of the porcelain veneer initiating at the indentation site. Fatigue was an acceleration factor for all-ceramic systems, but not for the MCR system. The latter presented significantly higher reliability under mouth-motion cyclic mechanical testing.

Original languageEnglish (US)
Pages (from-to)1051-1056
Number of pages6
JournalJournal of Dental Research
Volume89
Issue number10
DOIs
StatePublished - Oct 2010

Fingerprint

Metal Ceramic Alloys
Ceramics
Crowns
Fatigue
Mouth
Dental Porcelain
Tooth Preparation
Reproduction
Water
zirconium oxide

Keywords

  • all-ceramic
  • dental ceramic
  • fatigue
  • metal ceramic retainers
  • single-crown

ASJC Scopus subject areas

  • Dentistry(all)

Cite this

Silva, N. R. F. A., Bonfante, E. A., Zavanelli, R. A., Thompson, V. P., Ferencz, J. L., & Coelho, P. (2010). Reliability of metalloceramic and zirconia-based ceramic crowns. Journal of Dental Research, 89(10), 1051-1056. https://doi.org/10.1177/0022034510375826

Reliability of metalloceramic and zirconia-based ceramic crowns. / Silva, N. R F A; Bonfante, E. A.; Zavanelli, R. A.; Thompson, V. P.; Ferencz, J. L.; Coelho, Paulo.

In: Journal of Dental Research, Vol. 89, No. 10, 10.2010, p. 1051-1056.

Research output: Contribution to journalArticle

Silva, NRFA, Bonfante, EA, Zavanelli, RA, Thompson, VP, Ferencz, JL & Coelho, P 2010, 'Reliability of metalloceramic and zirconia-based ceramic crowns', Journal of Dental Research, vol. 89, no. 10, pp. 1051-1056. https://doi.org/10.1177/0022034510375826
Silva NRFA, Bonfante EA, Zavanelli RA, Thompson VP, Ferencz JL, Coelho P. Reliability of metalloceramic and zirconia-based ceramic crowns. Journal of Dental Research. 2010 Oct;89(10):1051-1056. https://doi.org/10.1177/0022034510375826
Silva, N. R F A ; Bonfante, E. A. ; Zavanelli, R. A. ; Thompson, V. P. ; Ferencz, J. L. ; Coelho, Paulo. / Reliability of metalloceramic and zirconia-based ceramic crowns. In: Journal of Dental Research. 2010 ; Vol. 89, No. 10. pp. 1051-1056.
@article{7d9bbd50857e4c05858391b18b842c11,
title = "Reliability of metalloceramic and zirconia-based ceramic crowns",
abstract = "Despite the increasing utilization of all-ceramic crown systems, their mechanical performance relative to that of metal ceramic restorations (MCR) has yet to be determined. This investigation tested the hypothesis that MCR present higher reliability over two Y-TZP all-ceramic crown systems under mouth-motion fatigue conditions. A CAD-based tooth preparation with the average dimensions of a mandibular first molar was used as a master die to fabricate all restorations. One 0.5-mm Pd-Ag and two Y-TZP system cores were veneered with 1.5 mm porcelain. Crowns were cemented onto aged (60 days in water) composite (Z100, 3M/ESPE) reproductions of the die. Mouth-motion fatigue was performed, and use level probability Weibull curves were determined. Failure modes of all systems included chipping or fracture of the porcelain veneer initiating at the indentation site. Fatigue was an acceleration factor for all-ceramic systems, but not for the MCR system. The latter presented significantly higher reliability under mouth-motion cyclic mechanical testing.",
keywords = "all-ceramic, dental ceramic, fatigue, metal ceramic retainers, single-crown",
author = "Silva, {N. R F A} and Bonfante, {E. A.} and Zavanelli, {R. A.} and Thompson, {V. P.} and Ferencz, {J. L.} and Paulo Coelho",
year = "2010",
month = "10",
doi = "10.1177/0022034510375826",
language = "English (US)",
volume = "89",
pages = "1051--1056",
journal = "Journal of Dental Research",
issn = "0022-0345",
publisher = "SAGE Publications Inc.",
number = "10",

}

TY - JOUR

T1 - Reliability of metalloceramic and zirconia-based ceramic crowns

AU - Silva, N. R F A

AU - Bonfante, E. A.

AU - Zavanelli, R. A.

AU - Thompson, V. P.

AU - Ferencz, J. L.

AU - Coelho, Paulo

PY - 2010/10

Y1 - 2010/10

N2 - Despite the increasing utilization of all-ceramic crown systems, their mechanical performance relative to that of metal ceramic restorations (MCR) has yet to be determined. This investigation tested the hypothesis that MCR present higher reliability over two Y-TZP all-ceramic crown systems under mouth-motion fatigue conditions. A CAD-based tooth preparation with the average dimensions of a mandibular first molar was used as a master die to fabricate all restorations. One 0.5-mm Pd-Ag and two Y-TZP system cores were veneered with 1.5 mm porcelain. Crowns were cemented onto aged (60 days in water) composite (Z100, 3M/ESPE) reproductions of the die. Mouth-motion fatigue was performed, and use level probability Weibull curves were determined. Failure modes of all systems included chipping or fracture of the porcelain veneer initiating at the indentation site. Fatigue was an acceleration factor for all-ceramic systems, but not for the MCR system. The latter presented significantly higher reliability under mouth-motion cyclic mechanical testing.

AB - Despite the increasing utilization of all-ceramic crown systems, their mechanical performance relative to that of metal ceramic restorations (MCR) has yet to be determined. This investigation tested the hypothesis that MCR present higher reliability over two Y-TZP all-ceramic crown systems under mouth-motion fatigue conditions. A CAD-based tooth preparation with the average dimensions of a mandibular first molar was used as a master die to fabricate all restorations. One 0.5-mm Pd-Ag and two Y-TZP system cores were veneered with 1.5 mm porcelain. Crowns were cemented onto aged (60 days in water) composite (Z100, 3M/ESPE) reproductions of the die. Mouth-motion fatigue was performed, and use level probability Weibull curves were determined. Failure modes of all systems included chipping or fracture of the porcelain veneer initiating at the indentation site. Fatigue was an acceleration factor for all-ceramic systems, but not for the MCR system. The latter presented significantly higher reliability under mouth-motion cyclic mechanical testing.

KW - all-ceramic

KW - dental ceramic

KW - fatigue

KW - metal ceramic retainers

KW - single-crown

UR - http://www.scopus.com/inward/record.url?scp=78049246693&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=78049246693&partnerID=8YFLogxK

U2 - 10.1177/0022034510375826

DO - 10.1177/0022034510375826

M3 - Article

C2 - 20660796

AN - SCOPUS:78049246693

VL - 89

SP - 1051

EP - 1056

JO - Journal of Dental Research

JF - Journal of Dental Research

SN - 0022-0345

IS - 10

ER -